MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Denka Neoprene 571 Copolymer of chloroprene and sulfur
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Chlorosulfonated Polyethylene Rubber

Material Notes: DuPont™ Neoprene 571 liquid dispersion contains a high modulus copolymer of chloroprene and sulfur made in an anionic colloidal system.

Main Features

  • High Tensile Strength
  • High Modulus Films
  • Cured films made from Neoprene 571 are characterized by high strength in addition to good hot oil resistance and low permanent set.

Suggested End Uses

  • Dipped goods
  • Elasticized aluminous cement
  • Industrial coatings
  • Cord adhesives

Denka Performance Elastomer LLC has acquired the Neoprene product line from DuPont Performance Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccLiquid Dispersion
 1.23 g/ccPolymer
Solids Content 50 %
pH >= 12
@Temperature 25.0 °C
 
Descriptive Properties
Compounding StabilityGood
Emulsifying AgentPotassium Rosinate
Freeze/Thaw StabilityNot stable
Mechanical StabilityGood
Storage StabilityGood

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Denka Neoprene 671A Polychloroprene
Denka Neoprene 842A Polychloroprene
Denka Neoprene 750 Copolymer of chloroprene and 2,3,dichloro-1,3,-butadiene
Denka Neoprene GNA Polychloroprene
Natural Rubber, Not Vulcanized (NR, IR, Polyisoprene)

PDVC9796 / 170437

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.