MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
M Cubed Technologies SSC-FG Reaction-Bonded Silicon Carbide, Fine-Grained
Categories: Ceramic; Carbide; Ceramic Matrix Composite

Material Notes: Fine-grained reaction-bonded SiC. Used for mechanical seals and other SiC applications that require a high surface finish/tight tolerances. Si content can be tailored for the application.

Information provided by M Cubed Technologies, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.00 g/ccASTM C135
 
Mechanical PropertiesOriginal ValueComments
Knoop Microhardness 1080
@Load 2.00 kg
kg/mm2; ASTM C1326
Modulus of Elasticity 330 GPaASTM E494
Flexural Strength 350 MPaASTM C1161
Poissons Ratio 0.18ASTM E494
Fracture Toughness 4.00 MPa-m½ASTM C1421
Shear Modulus 140 GPaCalculated
 
Thermal PropertiesOriginal ValueComments
CTE, linear 3.00 µm/m-°C
@Temperature 25.0 - 100 °C
ASTM E831
Thermal Conductivity 150 W/m-KASTM E1461
 
Descriptive Properties
MatrixSiC
Particle ReinforcementSiC
Vol. % Reinforcement70

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silicon Carbide, Reaction-Bonded, SiSiC
COI Ceramics Nextel™ AS-N720 Oxide Ceramic Matrix Composite, Aluminosilicate
COI Ceramics Sylramic™ S400 Silicon Carbide Ceramic Matrix Composite, Carbon
M Cubed Technologies HSC-702 Aluminum-toughened Reaction Bonded Silicon Carbide
COI Ceramics Nextel™ AS-N312 Oxide Ceramic Matrix Composite, Aluminosilicate

NMCUBE05 / 99805

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.