MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DayGlo ZQ Pigments ZQ-11 Aurora Pink
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have larger particle size to reduce dusting.

Applications:

  • Polyethylene
  • Polypropylene
  • Polystyrene
  • ABS
  • Ionomer
  • PA (Nylon)
  • Polycarbonate
  • Acrylic
  • Rigid PVC
  • Urethane

Key Words: Pigment; Colorant
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/cc
Particle Size 20 - 60 µm
 
Thermal PropertiesOriginal ValueComments
Melting Point 248 - 275 °F
Maximum Service Temperature, Air 575 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature >= 350 °F
 
Descriptive Properties
ColorAurora Pink

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik POLYTREND® 850-001 Colorant
Evonik G-P-D® 824-0009 General Purpose Dispersion
Evonik AQUASPERSE® II 877-0019 Color Dispersion
GEHR Plastics PVC-U Polyvinylchloride
Inovyn 260RF Polyvinyl Chloride General Purpose - Rigid

PDAYGLO07 / 29548

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.