MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

NaturePlast NPW SHE 231 Biopolyester
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: General Properties: The NPW SHE range consists of a set of Biocomposites which can be produced from oil based as well as biobased or biodegradable polymers. The by-products used here as fillers are waste material from shells or kernels from different sources.

Applications:
Process:

  • Primarily injection molding
  • Adaptable to other processes
Markets:
  • Rigid secondary packaging
  • Regular consumption goods
  • Technical parts
  • Agriculture / horticulture
  • Cosmetic / luxury
Properties:
  • Partially to totally biobased
  • Some of them are biodegradable and compostable
  • Rigid
  • Natural appearance

Information provided by NaturePlast Bioplastics Experts

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 17.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
17.3 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 5.0 %5.0 %ISO 527
Tensile Modulus 1.67 GPa242 ksiISO 527
Charpy Impact Unnotched 1.27 J/cm²6.04 ft-lb/in²ISO 179
 
Descriptive Properties
FillerRice husk
Filling Rate0.3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNATPLAS058 / 285507

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.