TAIPOL® 3206 is a Blend of linear SBS triblock and SB diblock copolymer with 29% styrene content. The product exhibits the following characteristics: - Low molecular weight
- Easy processing
- Good solubility in common adhesive solvent and non-polar solvent
- Mainly for shoe soles, adhesives(HMA), asphalt
Information provided by TSRC Corporation |