MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Copper Alloy (CW103C), UNS C17540, TF00 Temper, Forgings
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Precipitation Hardened

Fabrication Properties: Excellent Suitability – Capacity for Being Cold Worked; Good Suitability – Soldering, Brazing, Spot Weld, Seam Weld, Butt Weld, Capacity for Being Hot Formed; Fair Suitability – Gas Shielded Arc Welding, Coated Metal Arc Welding

Typical Uses: Welding and Brazing Components; Plunger tips, die casting

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.80 g/cc0.318 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 9595
Tensile Strength 827 MPa120000 psiTypical
 689 - 965 MPa100000 - 140000 psi
Elongation at Break 10 - 14 %10 - 14 %
Tensile Modulus 135 GPa19600 ksi
Modulus of Rigidity 51.97 GPa7538 ksiCalculated
Poissons Ratio 0.300.30
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000380 ohm-cm0.00000380 ohm-cm45% IACS
Magnetic Permeability 1.01.0
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.6 µm/m-°C
@Temperature 20.0 - 300 °C
9.80 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 19.5 W/m-K135 BTU-in/hr-ft²-°F
Melting Point 1030 - 1079 °C1880 - 1975 °F
Solidus 1030 °C1880 °F
Liquidus 1079 °C1975 °F
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 0.40 - 0.70 %0.40 - 0.70 %
Cobalt, Co 0.80 - 1.3 %0.80 - 1.3 %
Copper, Cu 96.3 - 98 %96.3 - 98 %As Balance
Iron, Fe <= 0.20 %<= 0.20 %
Nickel, Ni 0.80 - 1.3 %0.80 - 1.3 %
Silicon, Si <= 0.20 %<= 0.20 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC17540x2 / 291607

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.