Description: TIPPLEN K 850 is a bimodal, high molecular weight impact copolymer polypropylene for extrusion. Applications: TIPPLEN K 850 is applicable for extrusion of pipes, corrugated pipes, and fittings, tough sheet for industrial applications and thermoforming trays for storage in refrigerator. (1) Average mechanical property values of several measurements carried out on standard injection-molded test specimens prepared in accordance with ISO 294-1. Information provided by Molgroup Chemicals |