MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Melos Mecoline IS RDX 5243 F Radiation cross-linkable, flame retardant compound for insulation and sheathing
Categories: Polymer; Thermoplastic

Material Notes: Radiation cross-linkable, flame retardant compound for insulation and sheathing applications

Compound class: Insulation / sheathing

Compound category: RDX

Flame retardant: Halogenated

Standards: VG 95218, Part 24 (Type K), Part 25 (Type G ) Part 27 (Type B), Part 28 (Type A and D)

Typical applications: System cabling for military vehicles, aerospace, sensor technology, engine & transformer construction, automotive motor compartments and industrial automation and process controls.

Features: Flame retardant; Low smoke; Oil resistant; Abrasion resistant; High temperature resistant; Flexible; Flexible at low temperatures

Information provided by Melos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³pressed plaques; DIN EN ISO 1183-1A
Melt Flow 4.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.3 g/10 min
@Load 4.76 lb,
Temperature 374 °F
DIN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 2828pressed plaques; DIN ISO 7619-1
Tensile Strength >= 10.0 MPa>= 1450 psiextruded tapes; IEC 60811-501
 19.0 MPa2760 psicross-linked plaques or tapes, 130kGy; IEC 60811-501
Elongation at Break 400 %400 %cross-linked plaques or tapes, 130kGy; IEC 60811-501
 >= 600 %>= 600 %extruded tapes; IEC 60811-501
 >= 30 %
@Temperature -50.0 °C
>= 30 %
@Temperature -58.0 °F
cross-linked plaques or tapes; IEC 60811-505
 >= 150 %
@Temperature -40.0 °C
>= 150 %
@Temperature -40.0 °F
cross-linked plaques or tapes; IEC 60811-505
 10 %
@Temperature 200 °C,
Time 900 sec
10 %
@Temperature 392 °F,
Time 0.250 hour
Hot set test, Residual, 0.2 Mpa; IEC 60811-507
 25 %
@Temperature 200 °C,
Time 900 sec
25 %
@Temperature 392 °F,
Time 0.250 hour
Hot set test, under load, 0.2 Mpa; IEC 60811-507
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmpressed plaques; ASTM D 257
Dielectric Constant 7.8
@Frequency 50 Hz
7.8
@Frequency 50 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm508 kV/inpressed plaques; ASTM D 2671
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 170 - 180 °C338 - 356 °FTool
 190 °C374 °FMaximum mass temperature
Zone 1 150 - 160 °C302 - 320 °F
Zone 2 160 - 170 °C320 - 338 °F
Zone 3 165 - 175 °C329 - 347 °F
Zone 4 170 - 180 °C338 - 356 °F
Zone 5 170 - 180 °C338 - 356 °F
Adapter Temperature 170 - 180 °C338 - 356 °F
Head Temperature 170 - 180 °C338 - 356 °F
Drying Temperature 50.0 °C122 °F
Dry Time 3.00 hour3.00 hour
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) 28 %28 %pressed plaques; ASTM D 2863 A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMELOS047 / 296154

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.