MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Westlake 1230S PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Molded

Material Notes: Westlake PVC 1230S resin is a medium molecular weight homopolymer designed primarily for the extrusion of rigid products.

Information provided by Westlake Chemical Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.560 g/cc0.0202 lb/in³ASTM D1895
Particle Mesh Size 40 Mesh40 Mesh99.9% min; ASTM D1921
 200 Mesh200 Mesh4.0% max; ASTM D1921
Viscosity Measurement 0.900.90Inherent; ASTM D5225
 2.2
@Temperature 25.0 °C
2.2
@Temperature 77.0 °F
Relative (1.0% in Cyclohexanone)
Collected Volatile Condensable Material <= 0.20 %<= 0.20 %
 
Descriptive Properties
K-Value66

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Colorite Polymers 2019 Rigid PVC
Colorite Polymers 2018 Rigid PVC
Colorite Polymers 2010 Rigid PVC
Colorite Polymers 2007UV Rigid PVC
Colorite Polymers 2007NAT Rigid PVC

PWESG057 / 72703

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.