MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Honeywell 508B Refrigerant
Categories: Fluid

Material Notes: A non-ozone depleting azeotrope of R-23 and R-116 used to replace R-13 and R-503 in the low stage of cascade systems. For new equipment and retrofits.

Chemical Name: Trifluoromethane, Hexafluoroethane

Chemical Notation: CHF3, C2F6

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc
@Temperature -1.11 °C
0.0462 lb/in³
@Temperature 30.0 °F
Saturated Liquid
Molecular Weight 95.4 g/mol95.4 g/mol
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 37.88 bar28410 torr
Critical Temperature 11.827 °C53.289 °FASTM D1231
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.26 J/g-°C
@Temperature -1.11 °C
0.300 BTU/lb-°F
@Temperature 30.0 °F
Heat of Liquid
 0.586 J/g-°C
@Pressure 0.101 MPa,
Temperature -1.11 °C
0.140 BTU/lb-°F
@Pressure 14.7 psi,
Temperature 30.0 °F
Heat of Vapor @ Constant Pressure
Boiling Point -87.39 °C
@Pressure 0.101 MPa
-125.3 °F
@Pressure 14.7 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zinc, Zn
Aluminum, Al

PHONWL001 / 179546

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.