MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Momentive Performance Materials GE Silicones IGS3103 Silicone Insulating Glass Sealant
Categories: Polymer; Thermoset; Silicone

Material Notes: IGS3103 is a single-component, high strength, silicone sealant which is an excellent candidate to consider for use as a secondary seal in insulating glass construction. IGS3103 is supplied as a paste and upon dispensing, reacts with atmospheric moisture to produce a durable, formed-in-place silicone rubber sealant. Performance: Silicone Durability, High Modulus, Low VOC Content, Structural Capacity, Thermal Stability in Cured State, Specifications.

Applications: Strong Adhesion, Fast Curing, High Performance Rheological Characteristics, Low Sag or Slump.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccUncured.
Volatile Organic Compounds (VOC) Content 20 g/l20 g/lUncured.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3030ASTM D2240
Tensile Strength, Ultimate 3.10 MPa450 psiASTM D2240
Elongation, Ultimate 400 %400 %ASTM D412
Peel Strength 7.01 kN/m40.0 pliASTM C794
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -48.3 °C-55.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 - 4320 min24.0 - 72.0 hourFull Cured. 1/4" deep section.
 1440 min
@Temperature 24.0 °C
24.0 hour
@Temperature 75.2 °F
1/4" deep section.
Tack-Free Time 30.0 min0.500 hourASTM C679
Working Life 20.0 min20.0 min
 
Descriptive Properties
AppearancePaste
Application Rate400 grams/minuteMPM E-56
ColorBlackUncured.
Consistency / Sag0.1” max.
Silicone Content (%)100Uncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOMEN9924 / 265734

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.