MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Plastcom SLOVAMID 6 GF 35 FRC 5 PA6 reinforced with 35% glass fibre, with flame retardant  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled; Nylon 6, Glass Fiber Filled, Flame Retardant

Material Notes: PA 6 for injection moulding, chemically reinforced with 35 % glass fibre, with halogen free flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 750°C, CTI 600. Application for the electrical industry: protectors, coil forms, covers, terminals. Delivered in natural mode and in the full RAL color scale.

Packaging, transport, stocking: The product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.

Information Provided by Plastcom spol. s r.o.

Key Words: Polyamide 6 (PA6)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/cc
Linear Mold Shrinkage 0.0040 cm/cm
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 125 MPa
Elongation at Break 2.5 %
Tensile Modulus 12500 MPa
Flexural Strength 175 MPa
Flexural Modulus 7500 MPa
Charpy Impact Unnotched 33.0 kJ/m²
@Temperature -20.0 °C
 35.0 kJ/m²
@Temperature 23.0 °C
Charpy Impact, Notched 3.70 kJ/m²
@Temperature -20.0 °C
 3.80 kJ/m²
@Temperature 23.0 °C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cm
Surface Resistance 1.00e+15 ohm
Dielectric Strength 60.0 kV/mm
Comparative Tracking Index 600 V
 
Thermal PropertiesOriginal ValueComments
Melting Point 222 °C
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
Vicat Softening Point 210 °C
Flammability Test 3.0
@Thickness 1.60 mm
Glow Wire Test 750 °C
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 270 °C
Mold Temperature 50.0 - 70.0 °C
Drying Temperature 80.0 °C
Dry Time 4 hour
Moisture Content 0.15 %
Injection Pressure 70.0 - 100 MPa

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plastcom SLOVAMID 6 GF 35 TS Polyamide 6, 35% Glass Fiber, Thermal Stabilization
Albis Plastics Polyamide 6 PA 45/1 GF 35 , 35% Glass Fiber, Conditioned
Albis Plastics Polyamide 6 PA 45/1 GF 35 , 35% Glass Fiber, DAM
Avient Gravi-Tech™ GRV-NY-035-SS-GF-BLK Polyamide 6 (Nylon 6)
Avient Nymax™ GF 604 35 HS Black 13 Polyamide 6 (Nylon 6)

PPLACO518 / 122719

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.