MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Aperam Resistohm® 135 Resistant Alloys Iron-Chromium-Aluminium Alloys
Categories: Metal; Ferrous Metal

Material Notes: Resistohm 135 is a ferritic alloy of the FeCrAl family, which can be used as heating element of resistance up to 1200°C. Resistohm 135 must be used in a dry environment in order to avoid rust because this is not a stainless alloy. Elements realized in Resistohm 135 have an excellent life time in a sulphurous environment, and particularly when atmosphere is also oxidizing. A preoxidation (2 hours at more than 1000°C out in the open air) is necessary when Resistohm 135 must operate in a reducing atmosphere. The white-grey aluminum coat formed during the oxidation heat treatment preserves the wire or the ribbon of the future chemical attacks. Resistohm 135 is normally used in top cookers with ceramics, pottery furnaces elements, and tubular elements. Because of its resistance to carbonaceous atmospheres, Resistohm 135 is chosen for the production of cigarette lighters and fuel burners elements.

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.25 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 230
Tensile Strength 750 MPa
Tensile Strength, Yield 550 MPa
Elongation at Break >= 18 %on 100 mm
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.000135 ohm-cmTemperature coefficient = 0.000070/°C from 20 - 100°C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.0 µm/m-°C
@Temperature 20.0 - 1000 °C
Thermal Conductivity 16.5 W/m-K
@Temperature 120 °C
Melting Point 1500 °C
Maximum Service Temperature, Air 1200 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 4.5 %
Chromium, Cr 20 %
Iron, Fe 75.5 %
 
Descriptive Properties
Creeping point1at 1000°C
 6at 800°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aperam Resistohm® 125 Resistant Alloys Iron-Chromium-Aluminium Alloys
Titanium 11 (Ti-6Al-2Sn-1.5Zr-1Mo-0.35Bi-0.1Si), Aged
AISI 1018 Steel, cold drawn
Special Metals Nitinol Superelastic Ni-Ti alloy
Titanium Ti-11.5Mo-6Zr-4.5Sn, ST 720°C, Aged 495°C

NPERA087 / 194876

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.