System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Dowhon DHF-50611NCL FFKM, Copolymer, Oring, Gasket
Categories:
Polymer
;
Thermoset
;
Fluoropolymer, TS
;
Thermoset Fluoroelastomer
Material Notes:
Property: very low hardness, good mold release, hot tear resistance
Information provided by SICHUAN DOWHON NEW MATERIALS CO., LTD.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.83
g/cc
1.83
g/cc
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
48
48
45
@Temperature 150 °C,
Time 252000 sec
45
@Temperature 302 °F,
Time 70.0 hour
OIL 903
48
@Temperature 250 °C,
Time 252000 sec
48
@Temperature 482 °F,
Time 70.0 hour
Aging
Tensile Strength
10.0
MPa
1450
psi
8.27
MPa
@Temperature 150 °C,
Time 252000 sec
1200
psi
@Temperature 302 °F,
Time 70.0 hour
OIL 903
10.99
MPa
@Temperature 250 °C,
Time 252000 sec
1594
psi
@Temperature 482 °F,
Time 70.0 hour
Aging
Elongation at Break
280 %
280 %
216.44 %
@Temperature 250 °C,
Time 252000 sec
216.44 %
@Temperature 482 °F,
Time 70.0 hour
Aging
284.76 %
@Temperature 150 °C,
Time 252000 sec
284.76 %
@Temperature 302 °F,
Time 70.0 hour
OIL 903
Compression Set
30 %
@Temperature 200 °C,
Time 252000 sec
30 %
@Temperature 392 °F,
Time 70.0 hour
ASTM D395 Method B
Thermal Properties
Metric
English
Comments
Minimum Service Temperature, Air
-18.0
°C
-0.400
°F
TR10
Brittleness Temperature
-30.0
°C
-22.0
°F
Descriptive Properties
Color
black
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PDOWHON055 / 315967
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.