MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Prism® CM-200 Polyurethane Solid RIM, MDI-based 2-Component Liquid System
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Solid RIM

Material Notes: Characterization: Prism CM-200 solid polyurethane system is used in the reaction injection molding (RIM) process.

Properties / Applications: Prism CM-200 solid polyurethane system incorporates an internal mold release (IMR) and is supplied as two reactive components: Component A is a polymeric diphenylmethane diisocyanate (MDI), and Component B is a polyol blend. The Prism CM-200 system has a UL94 flammability rating of V-0/5VA and is used for applications in the electronic, equipment housing and appliance markets. The applications typically take advantage of the material ’s strength, excellent surface finish, and large-part capability. As with any product, use of the Prism CM-200 system in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ASTM D792
Linear Mold Shrinkage 0.0070 - 0.0090 cm/cm0.0070 - 0.0090 in/inBayer Test
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575ASTM D2240
Tensile Strength, Ultimate 48.0 MPa6960 psiASTM D638/D412
Elongation at Break 9.0 %9.0 %ASTM D638/D412
Flexural Yield Strength 76.0 MPa11000 psiat 5% strain; ASTM D790
Flexural Modulus 2.03 GPa294 ksiASTM D790
Izod Impact, Unnotched 4.30 J/cm8.06 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 5.20e+14 ohm-cm5.20e+14 ohm-cmASTM D257
Surface Resistance 7.90e+14 ohm7.90e+14 ohmASTM D257
Dielectric Constant 3.07
@Frequency 1e+6 Hz
3.07
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 19.0 kV/mm483 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C221 °FASTM D648
UL RTI, Electrical  85.0 °C
@Thickness 6.35 mm
185 °F
@Thickness 0.250 in
UL746B
 90.0 °C
@Thickness 3.20 mm
194 °F
@Thickness 0.126 in
UL746B
UL RTI, Mechanical with Impact  75.0 °C
@Thickness 6.35 mm
167 °F
@Thickness 0.250 in
UL746B
 80.0 °C
@Thickness 3.20 mm
176 °F
@Thickness 0.126 in
UL746B
UL RTI, Mechanical without Impact  85.0 °C
@Thickness 6.35 mm
185 °F
@Thickness 0.250 in
UL746B
 90.0 °C
@Thickness 3.20 mm
194 °F
@Thickness 0.126 in
UL746B
Flammability, UL94 5VA5VAUL94
 V-0
@Thickness 3.18 mm
V-0
@Thickness 0.125 in
UL94
 
Processing PropertiesMetricEnglishComments
Mold Temperature 65.0 - 75.0 °C149 - 167 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Materia Proxima® HPR 2100 Polydicyclopentadiene Thermoset Resin
Overview of materials for Phenolic, Novolac, Heat Resistant Grade, Filled
Chi Mei Polylac® PA-746 ABS - High Flow
Overview of materials for Thermoset Polyester Glass Filled BMC
A. Schulman Premi-Glas® 2100-22CRSX Polyester BMC

PB2P00 / 26635

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.