MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Lotte Advanced Materials Titanvene™ HD5740UA HDPE, Injection Molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Titanvene™ HD5740UA is an ultra violet (UV) light stabilized high density polyethylene copolymer with a narrow molecular weight distribution, specially developed for injection molding of heavy duty articles. Titanvene™ HD5740UA is characterized by its high rigidity, high impact resistance (especially for low temperature) and high weathering resistance.

Applications: Titanvene™ HD5740UA is designed for: Caps and Closure; Large dustbin and pails; Fish crates/pallet boxes; Technical parts

Information provided by Lotte Advanced Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.955 g/ccISO 1183 Method D
ESCR 10% Igepal® 9.00 hourCondition B, F50; ASTM D1693
Melt Flow 4.00 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133 Condition 7
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 66.0ISO 868 Type D
Tensile Strength, Yield 275 kg(f)/cm²Type 2 Speed C; ISO/R 527
Elongation at Break 2200 %Type 2 Speed C; ISO/R 527
Flexural Modulus 16300 kg(f)/cm²ISO 178
Charpy Impact, Notched 9.00 kJ/m²ISO 179 Type 1 Notch A
 
Thermal PropertiesOriginal ValueComments
Melting Point 132 °CISO 3146 Method C
Vicat Softening Point 127 °CISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLOTT9590 / 326072

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.