MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond EP77M-FMed Two component, silver conductive epoxy adhesive for medical applications
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, Electrically Conductive

Material Notes: Master Bond EP77M-FMed is a two component, silver filled, electrically conductive adhesive for high performance bonding formulated to cure very rapidly at room temperature. Unlike the majority of two part, silver conductive epoxy systems, EP77M-FMed has a one to one mix ratio, by weight or volume. It will set up at ambient temperatures within 15-20 minutes even when mixed in very small amounts. Full cures usually take about 24 hours at room temperature. It is 100% reactive and does not contain any diluents or solvents. The volume resistivity of the cured system is a very low 10-3 ohm-cm. EP77M-FMed can be applied with minimal sagging or dripping, even on vertical surfaces. The high strength bonds are remarkably adaptable to thermal cycling and resistant to chemicals including water, most liquid sterilants and EtO sterilization. The service temperature range is -100°F to +250°F. Adhesion to metals, glass, ceramics, vulcanized rubbers and many plastics is excellent. Parts A and B are both colored silver. Master Bond EP77M-FMed adhesive is widely used in medical device applications.

Product Advantages:

  • Convenient mixing: one to one by weight or volume
  • Contains no solvents or diluents
  • Easy application: contact pressure only required for cure; adhesive spreads evenly and smoothly
  • Exceptionally fast room temperature cure
  • Very low volume resistivity
  • Superior toughness and ability to withstand thermal cycling
Key Features:
  • Exceptionally low volume resistivity
  • Convenient one to one mix ratio
  • Fast fixture time at room temperature
  • Passes ISO 10993-5

Information provided by Master Bond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 40 - 5040 - 50
Tensile Strength 13.8 - 20.7 MPa2000 - 3000 psi
Tensile Modulus 1.72 - 2.07 GPa250 - 300 ksi
Adhesive Bond Strength 3.45 - 4.83 MPa500 - 700 psiTensile lap shear, Al to Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 0.0010 ohm-cm>= 0.0010 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.44 - 1.73 W/m-K10.0 - 12.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 135 °C275 °F
Minimum Service Temperature, Air -73.0 °C-99.4 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hour
Working Life 10.0 - 15.0 min10.0 - 15.0 minWorking Life; 20 gram batch
Shelf Life 3.00 - 6.00 Month3.00 - 6.00 Month
 
Descriptive Properties
Mixing ratio1:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASTM641 / 268829

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.