MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Vyncolit Neopreg Kinel® SK80 L8G Glass Fiber Reinforced Molding Compound
Categories: Polymer; Thermoset; Epoxy; Epoxy Molding Compound; Filled/Reinforced Thermoset

Material Notes: Epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited for over molding and manufacturing of large commutators.

Information provided by Sumitomo Bakelite North America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.590 g/ccISO 60
Density 1.79 g/ccISO 1183
Water Absorption 0.050 %ISO 62
Linear Mold Shrinkage 0.0011 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 119 MPaISO 527-1
Elongation at Break 0.70 %ISO 527-1
Tensile Modulus 19.0 GPaISO 527-1
Flexural Strength 255 MPaISO 178
Flexural Modulus 17.0 GPaISO 178
Compressive Strength 265 MPaISO 604
Charpy Impact, Notched 54.0 kJ/m²ISO 179-1
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 29.0 kV/mmIEC 60243-1
Dissipation Factor 0.019IEC 60250
Comparative Tracking Index 225 VIEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 9.60 µm/m-°CTMA
CTE, linear, Transverse to Flow 57.0 µm/m-°CTMA
Thermal Conductivity 0.490 W/m-KASTM E1461
Glass Transition Temp, Tg 195 °C
Shrinkage -0.0200 %Post Shrinkage; ISO 2577
 
Descriptive Properties
ColorDark Grey
Molding MethodCompression
 Injection
 Transfer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Vyncolit Vyntec® CF8050 Carbon Fiber Reinforced Phenolic
Vyncolit Neopreg Kinel® SK4504 S12 Carbon Reinforced Molding Compound
Vyncolit Neopreg Kinel® SK4502 S8 Carbon Reinforced Molding Compound
Vyncolit Vyntec® CF8131 Carbon Fiber Reinforced Phenolic
Vyncolit X7012 Glass Fiber Reinforced Novolac Phenolic

PVYNCN942 / 142717

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.