MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials Pearlthane® D91F88 Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP

Material Notes: Type: Pearlthane® D91F88 is an aliphatic-based thermoplastic polyurethane.

Main Application : Extrusion

Special features : Outstanding abrasion loss, excellent color stability upon weather exposure. High quality film and good transparency.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/ccISO 2781
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 88ISO 868
Tensile Strength, Yield 3770 psiISO 527-2/5A/500
Elongation at Break 415 %ISO 527-2/5A/500
50% Modulus 0.00600 GPa
@Strain 50 %
ISO 527-2/5A/500
100% Modulus 0.798 ksi
@Strain 100 %
ISO 527-2/5A/500
300% Modulus 2.321 ksi
@Strain 300 %
ISO 527-2/5A/500
Tear Strength 102 kN/mISO 34-1B
Abrasion 35[mm^3]; ISO 4649-A
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 48.0 °CISO 306
 
Processing PropertiesOriginal ValueComments
Zone 1 165 - 175 °C
Zone 2 175 - 185 °C
Zone 3 185 - 195 °C
Zone 4 190 - 200 °C
Adapter Temperature 190 - 200 °C5
Die Temperature 190 - 200 °C6
 190 - 200 °CTIP, 7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials Pearlthane® D91F65D Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials Pearlcoat® Activa D198K Thermoplastic Polyurethane Elastomer

PMES82 / 101414

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.