MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

A. Schulman Lucent TPO-10T Thermoplastic Polyolefin, 10% Mineral Filled
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Melt Flow Adjustable for Application
Add "U" for UV Stabilized
Add "H" for Heat Stabilized

Information provided by Lucent Polymers, Inc. Lucent was acquired by A. Schulman in 2015.

Key Words: TPO
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 g/cc0.980 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.013 cm/cm
@Thickness 3.17 mm
0.013 in/in
@Thickness 0.125 in
1/8" Section
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 21.0 MPa3050 psiASTM D638
Elongation at Break >= 100 %>= 100 %ASTM D638
Flexural Strength 29.0 MPa4210 psiASTM D790
Flexural Modulus 0.772 GPa112 ksiASTM D790
Izod Impact, Notched 9.99 J/cm
@Thickness 3.17 mm
18.7 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 41.0 °C106 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyplastic Armlen® PP MF 25-3-901 Polypropylene, 20% Mineral Filled
Teknor Apex Telcar® TL-2683B Thermoplastic Elastomer
Noble Polymers Ecobarrier™ 0712 Thermoplastic Olefin (TPO)
Formosa Plastics Formolene® 2706A Injection Molding RTPO Polypropylene
Borealis Daplen™ EE103AE TPO Compound

PLUCE106 / 90025

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.