MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SABIC NORYL PPX™ Resin PPX7115 Polyphenylene Ether + PP (PPE+PP) (Europe)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polypropylene (PP)

Material Notes: NORYL PPX™ 7115 resin is a non-reinforced alloy of polyphenylene ether (PPE) + polypropylene (PP). This injection moldable grade exhibits high modulus, high-temperature performance, excellent melt strength, impact resistance, hydrolytic and dimensional stability. NORYL PPX7115 resin is an excellent candidate for applications requiring high modulus and chemical resistance.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Low Warpage,High Impact Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.990 g/cc0.0358 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Viscosity 12 cP
@Load 5.00 kg,
Temperature 260 °C
12 cP
@Load 11.0 lb,
Temperature 500 °F
MVR cc/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 6060ISO 2039-2
Tensile Strength at Break 31.0 MPa4500 psi50 mm/min; ISO 527
Tensile Strength, Yield 35.0 MPa5080 psi50 mm/min; ISO 527
Elongation at Break 75 %75 %50 mm/min; ISO 527
Elongation at Yield 5.0 %5.0 %50 mm/min; ISO 527
Tensile Modulus 1.37 GPa199 ksi1 mm/min; ISO 527
Flexural Strength 51.0 MPa7400 psiyield, 2 mm/min; ISO 178
Flexural Modulus 1.52 GPa220 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 36.0 kJ/m²17.1 ft-lb/in²80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched NBNBEdgew 80*10*4 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 3.70 J/cm²17.6 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 114 °C237 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C181 °FEdgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 80.0 °C176 °FRate B/50; ISO 306
 85.0 °C185 °FRate B/120; ISO 306
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 260 - 290 °C500 - 554 °F
Zone 2 240 - 285 °C464 - 545 °F
Zone 3 250 - 290 °C482 - 554 °F
Melt Temperature 260 - 290 °C500 - 554 °FInjection Molding
Mold Temperature 40.0 - 60.0 °C104 - 140 °F
Drying Temperature 60.0 - 65.0 °C140 - 149 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82224 / 290171

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.