MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

NuSil CV-2289-1 Silicone, Two Part Adhesive and Sealant
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: General Purpose: Two Part Adhesive and Sealant

Comments: Pourable Elastomer

Cure system: Platinum

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 40000 cP40000 cPB
 60000 cP60000 cPA
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3030
Tensile Strength at Break 4.80 MPa696 psi
Elongation at Break 350 %350 %
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 37.6 kV/mm955 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 445 µm/m-°C247 µin/in-°F
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min
@Temperature 150 °C
0.250 hour
@Temperature 302 °F
Tack-Free Time 240 min4.00 hour
Working Life 30.0 min30.0 min
 
Descriptive Properties
ColorWhite
Mix Ratio1:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NuSil R1-2145 Silicone Two Part Sealing & Adhesive
NuSil CV-2680-12 Silicone, Film Adhesive

PNUSIL153 / 141877

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.