MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SEKISUI SPI KYDEX® 7200ST Thermoplastic
Categories: Polymer; Thermoplastic

Material Notes: Smoke and toxicity compliant aviation sheet

KYDEX® 7200ST is a high performance thermoplastic sheet designed for use in aviation interior applications where smoke and ABD0031 or BSS7239 toxicity compliance is required

KYDEX® 7200ST meets the flammability and smoke development requirements set forth in Federal Aviation Regulations (FAR) 25.853 paragraphs (a) and (d) Part V as well as the toxicity requirements for Airbus (ABD0031) and Boeing (BSS7239). Its wide processing window and ease of thermoforming makes it ideal for complex parts.

Suggested Applications:

  • Armrests
  • Tray tables
  • Kick panels
  • Trim parts

Features:

  • Meets flammability and smoke development requirements listed in FAR 25.853(a) and (d) Part V
  • Compliant to ABD0031 and BSS7239 toxicity specifications
  • Excellent formability and fabrication characteristics
  • Allows for tight tolerance control
  • Available in P3 - Velour Matte in thicknesses from 1.19 mm to 4.75 mm (0.047 in to 0.187 in)

Values based upon 0.125 in (3.18 mm) sheet unless otherwise specified.

Information provided by Sekisui Polymer Innovations

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.25 g/ccASTM D792
Moisture Absorption 0.160 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 112ASTM D785
Tensile Strength 53.5 MPaASTM D638
Tensile Modulus 2868 MPaASTM D638
Flexural Strength 87.6 MPaASTM D790
Flexural Modulus 2758 MPaASTM D790
Compressive Yield Strength 73.1 MPaASTM D695
Compressive Modulus 2718 MPaASTM D695
Ultimate Bearing Strength 246 MPaASTM D953
Bearing Yield Strength 27.6 MPa4% deflection; ASTM D953
Shear Strength 45.5 MPaASTM D732
Gardner Impact 46.9 JASTM D5420
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength >= 23.8 kV/mmoil; ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Transverse to Flow 28.6 µin/in-°FASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 212 °FUnannealed/Annealed; ASTM D648
 
Descriptive Properties
FlammabilityDmax<200FAR 25.853(d) Part V; NBS Smoke Density; all thicknesses
 PassABD-0031; Airbus Toxic Gas Generation; all thicknesses
 PassBSS 7239; Boeing Toxic Gas Generation; all thicknesses
 PassFAR 25.853(a)(i); Vertical Burn, 60 sec; all thicknesses
 PassFAR 25.853(a)(ii); Vertical Burn, 12 sec; all thicknesses

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SEKISUI SPI KYDEX® 430 ABS/PVC
SEKISUI SPI KYDEX® 4545 Thermoplastic
SEKISUI SPI KYDEX® 410 ABS/PVC
SEKISUI SPI KYDEX® 110 Polymer Alloy Sheet
SEKISUI SPI KYDEX® 100 Polymer Alloy Sheet

PSEKIS042 / 185867

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.