MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Michelman® Michem® Lube 103DI Anionic polyethylene emulsion
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: Anionic polyethylene emulsion

Usage: Michem® Lube 103DI is a wax emulsion additive which provides lubricity and mar resistance and is well suited for the glass and metal die industries.

Compatible with ingredients used in many industries, including: Automotive care products; Building materials; Can and coil coatings; Concrete; Cordage and twine; Deck stains and sealants; Die lubricants; Fiber sizings; Floor polishes; Furniture coatings; Glass; Gloves, balloons, footwear and mechanical seals; Inks; Packaging films; Pressure-sensitive adhesives; Textiles; Urethane foam and Varnishes

When manufactured in the USA product meets food contact regulations for:
Germany:
BfR Recommendation XIV (Restricted)

Food Contact Information when manufactured in the USA:
FDA:
175.105: Components of adhesives.
176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted)
176.180: Components of paper and paperboard in contact with dry foods.

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.970 - 0.990 g/cc0.970 - 0.990 g/cc
Volatiles 74.5 - 75.5 %74.5 - 75.5 %
pH >= 7.0>= 7.0Recommended pH of system
 8.2 - 9.28.2 - 9.2
Brookfield Viscosity <= 20 cP<= 20 cPSpindle # 1, rpm 60
 
Descriptive Properties
AppearanceAmber, translucent liquid
Emulsifier ChargeAnionic
Solids TypePolyethylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cymat A35620SC 020SS Stabilized Aluminum Foam
Evonik TEGO® Antifoam 5-27 Emulsion
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Autoclaved aerated concrete, 2.100 g/cc density
Autoclaved aerated concrete, 0.800 g/cc density

WMICHEL141 / 135058

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.