MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Master Bond EP19LV One Component Epoxy System
Categories: Polymer; Thermoset; Epoxy

Material Notes: Key Features:
  • Low viscosity
  • Impressive durability
  • Unlimited working life at room temperature
  • Superior temperature resistance properties
  • High physical strength profile
  • Excellent electrical insulator
Product Description: Master Bond EP19LV is a storage stable one component liquid epoxy resin system for durable, high performance adhesive/sealants, impregnants and liners. It feature remarkably long shelf life and excellent storage characteristics at ambient temperatures yet cures readily at elevated temperatures to a tough, strong and chemically resistant thermoset plastic. Low viscosity facilitates handling at ambient temperatures and is particularly desirable for impregnation applications. As EP19LV is 100% reactive and does not contain any solvents or diluents, shrinkage upon cure in minimal. Recommended cure conditions are 1.5-2 hours at 300°F (150°C), less at higher temperatures. The cured material has high physical strength properties (tensile strength more than 10,000 psi), is thermally stable (heat deflection temperature more than 280°F) and has superior electrical insulation properties (volume resistivity greater than 1015 ohm-cm) as well as remarkably good chemical resistance properties. EP19LV is widely used in the mechanical and in the electrical/electronic industries as an adhesive/sealant, impregnant for porous metals and nonmetals and as a high strength, chemically resistant liner. EP19LV can be used over the remarkably wide temperature range of -60°F to more than +300°F. It has a shelf life of more than 4 months when stored at 75°F and it can be extended to more than 6 months by storage at 40°F to 50°F.

Product Advantages:

  • Low viscosity assures convenient handling and easy processing
  • Superior thermal stability up to 300°F service
  • Remarkably good chemical resistance to water, inorganic acids, bases, salts and many organic solvents
  • Low odor and toxicity

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 500 - 600 cP
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 10200 psi
Elongation at Break 3.5 %
Tensile Modulus 340000 psi
Tensile Impact 0.410 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cm
Dielectric Constant 3.9
@Frequency 60 Hz
Dielectric Strength >= 790 V/mil
Dissipation Factor 0.0080
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °F
Heat Distortion Temperature 280 °F
Minimum Service Temperature, Air -60.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 - 1.50 min
@Temperature 149 °C
Shelf Life 4.00 Month
@Temperature <=23.9 °C
in original, unopened containers
 6.00 Month
@Temperature 7.22 - 10.0 °C
refrigerated
 
Descriptive Properties
ColorClear Amber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMASTM813 / 185406

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.