MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Covestro Bayhydrol® A 2601 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Water-reducible, hydroxyfunctional polyacrylate dispersion. In combination with aliphatic polyisocyanates for the formulation of waterborne two-component clearcoats and topcoats for general industrial and transportation coatings. Can also be used in combination with suitable melamine resins for the formulation of one-component coatings.

Properties / Applications: Primarily in combination with Bayhydur® 304, XP 2487/1 and Desmodur® N 3900 for air- and oven-drying industrial coatings. The cured coating film is hard, tough but flexible and exhibits high gloss, good filling power, good weather and light stability, good resistance to solvents and gasoline and rapid drying. Not recommended for clearcoat applications for wood.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccDIN EN ISO 2811
Volatiles 53 - 56 %53 - 56 %1g/1 ml toluene/1 h/125 °C; DIN EN ISO 3251
pH 7.0 - 8.07.0 - 8.01:4 in demineralized water; DIN ISO 976
Viscosity 1500 - 3000 cP1500 - 3000 cPD= approx. 40 s-1; DIN EN ISO 3219/A.3
 
Chemical PropertiesMetricEnglishComments
Acid Value 1010[mg KOH/g]; DIN EN ISO 2144
 
Descriptive Properties
Content3.9%Hydroxyl

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOVEST0156 / 201939

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.