MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF Gamma-Butyrolactone (GBL)
Categories: Fluid; Solvent

Material Notes: Formula: C4H6O2

CAS: 96-48-0

Description: GBL is a colorless, odorless liquid. It is miscible in water and with many organic solvent.

Synonyms: GBL, Butyrolactone, BLO, 1-Oxacyclopentan-2-one, 4-Butanolide, 4-Butyrolactone

Applications: Intermediate used in/as Crop protection agents, Photographic chemicals, Formulation aids, Wood preservative, Solvent, Foundry resins, Printing ink industry, Textile industry, Leather industry and Plastics processing

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/cc
Molecular Weight 86.1 g/mol
 
Thermal PropertiesOriginal ValueComments
Boiling Point 204 - 206 °C
Flash Point 100 °C
Ignition Temperature 455 °C
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.050 %DIN 51 777
 
Descriptive Properties
Assay>97.5%Area
Color<20APHA, DIN EN 1557
Composition1,4-Butanedio, Area<0.1%, STI 8460
 Acid Content<0.03%, STI 8461
 Methylbutyrolactone, Area<0.4%, STI 8460

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ethyl-(2-hydroxyethyl)aniline
BASF Hydroxypivalic Acid Neopentylglycolester (HPN
Resin Technology Group Fusion Debonder
BASF Isobutyleneoxide
BASF Hydroxybutyl Vinyl Ether

PBASG0883 / 132516

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.