MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sichuan Deyang Haton® hCF41 Polyphenylene Sulfide
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler

Material Notes: Injection molding, high strength

Information provided by Sichuan Deyang Chemical Co., LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.51 g/ccGB/T 1033.1-2008
Water Absorption 0.020 %GB/T 1034-2008
Linear Mold Shrinkage, Flow 0.0010 cm/cmGB/T 15585-1995
Linear Mold Shrinkage, Transverse 0.0019 cm/cmGB/T 15585-1995
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell L 110GB/T 3398.2-2008
Tensile Strength 188 MPaGB/T 1040.2-2006
Elongation at Break 0.80 %GB/T1040.2-2006
Flexural Strength 267 MPaGB/T 9341-2008
Flexural Modulus 23.1 GPaGB/T 9341-2008
Izod Impact, Notched (ISO) 7.20 kJ/m²GB/T 1843-2008
 
Electrical PropertiesOriginal ValueComments
Insulation Resistance 4.50e+7 ohmGB/T 10064-2006
 
Thermal PropertiesOriginal ValueComments
Melting Point 280 °CGBT/T 19466.3-2004
Deflection Temperature at 1.8 MPa (264 psi) 268 °CGB/T 1634.2-2004
Flammability, UL94 V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sichuan Deyang Haton® hGR31M1 Polyphenylene Sulfide
Sichuan Deyang Haton® hGR302 PPS / F4 Polyphenylene Sulfide
Sichuan Deyang Haton® hGC51 PPS / AE Polyphenylene Sulfide
Sichuan Deyang Haton® hFR81 Polyphenylene Sulfide
Sichuan Deyang Haton® hFR70 PPS / AR Polyphenylene Sulfide

PSICHU918 / 156159

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.