MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M 7218SA Screen Printable Polyester Performance Label Products with Structured Adhesive
Categories: Polymer; Adhesive

Material Notes: 3M™ Screen Printable Polyester Performance Label Products with Structured Adhesive are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label stocks utilize 3M™ Adhesive 350, which is designed to permanently bond to high and low surface energy plastics, textured and contoured surfaces, powder coatings, and slightly oily metals. With unique microchannels throughout the structured adhesive, air flows freely from between the adhesive and substrate. Hand applied labels go on smoothly and stay that way. Even when labels are used on injection-molded plastic parts, bubbles that form from plastic outgassing can be smoothed to regain a neat appearance for the graphic.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 27.9 microns1.10 milAdhesive
 50.8 microns2.00 milFacestock
 198 microns7.80 milLiner
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.421 kN/m2.40 pliHDPE, 180° Peel, 12"/min., 1" wide sample; TLMI Method
 0.543 kN/m3.10 pliPolypropylene, 180° Peel, 12"/min., 1" wide sample; TLMI Method
 0.543 kN/m3.10 pliPolycarbonate, 180° Peel, 12"/min., 1" wide sample; TLMI Method
 0.666 kN/m3.80 pliStainless Steel, 180° Peel, 12"/min., 1" wide sample; TLMI Method
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -29.0 °C-20.2 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 10.0 °C>= 50.0 °FApplication
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Adhesive Type350
Liner90# Embossed Polycoated

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM33670 / 168417

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.