MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Clax Italia AQuariA® Cast Acrylic
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Cast

Material Notes: AQuariA® Aquarium windows and made from Perclax® pure cast acrylic blocks, specifically produced, certified (PVHO-1) and guaranteed, for underwater use. This innovative material has been designed for the new, large private and public aquariums. AQuariA® pure cast acrylics, exhibit extreme purity and transparency, brightness, lightness and aging resistance, and availability in large acrylic blocks, with thicknesses up to 750 mm and sizes up to 9980×3050 mm.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccASTM D792
Water Absorption <= 0.2 %ASTM D570
Molecular Weight >= 3.00e+6 g/mol
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 815 kg(f)/cm²ASTM D638
Elongation at Break >= 5 %ASTM D638
Modulus of Elasticity >= 3.30 GPaASTM D638
Flexural Strength 120 MPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point >= 105 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49ASTM D542
Haze <= 0.5 %ASTM D1003
Transmission, Visible >= 92 %ASTM D1003
 
Descriptive Properties
Free Monomer<1%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acrylic, Cast
Hippe PMMA
Clax Italia Perclax® Cast Acrylic
LG Chemical HI855H PMMA, Impact Resistant Grade
Mitsubishi Rayon ACRYPET IR G504 001 PMMA Resin

PCLAX991 / 192234

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.