MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Semicosil® 960 RED Conformal Coating
Categories: Polymer; Thermoset; Silicone

Material Notes: SEMICOSIL® 960 RED is a RTV-1 amine cure silicone rubber dispersion that cures on contact with moisture in the air.

Special features:

  • Rapid cure
  • Excellent electrical properties
  • Excellent adhesion to many substrates
  • Available in clear or red
Application: SEMICOSIL® 960 RED is a conformal coating that forms a tough, rubbery film designed to protect electronic circuits from environmental influences.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccASTM D1475
Solids Content 65 %
Brookfield Viscosity 4000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 25ASTM D2240
Tensile Strength at Break 1.72 MPaASTM D412
Elongation at Break 300 %ASTM D412
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Dielectric Constant 2.7
@Frequency 1000 Hz
IEC 60250
Dielectric Strength 18.0 kV/mmIEC 60243
Dissipation Factor 0.00030
@Frequency 1000 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.180 W/m-K
Brittleness Temperature -45.0 °CASTM D746
Flash Point 21.0 °CASTM D93
 
Processing PropertiesOriginal ValueComments
Cure Time 168 hour
@Treatment Temp. 25.0 °C
50% RH
 
Descriptive Properties
Appearancered liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Semicosil® 960 CLEAR Conformal Coating

PWACK9421 / 204950

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.