MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Honeywell AClyn® 295P EAA copolymer
Categories: Polymer; Thermoplastic; Ethylene Acrylic Acid; Ionomer

Material Notes: Ionomer of an EAA copolymer, based on AC 540, which is 98% neutralized with Zinc. Zinc adds corrosion protection. Is a dispersing agent for color masterbatch in engineering and styrenic resin systems. Test

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 2400 cP
@Temperature 190 °C
2400 cP
@Temperature 374 °F
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.000.00
 
Thermal PropertiesMetricEnglishComments
Dropping Point 99.0 °C210 °FMettler
 
Descriptive Properties
Hardness1 dmmASTM D5
Product FormPastille

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Honeywell A-C® 5120 EAA copolymer
Honeywell AClyn® 201 EAA copolymer
Honeywell AClyn® 201A EAA copolymer
Honeywell AClyn® 295A EAA copolymer
Honeywell A-C® 5180 EAA copolymer

PHONWL091 / 179636

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.