MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Phillips 66 Syncon® Mist Oil, AGMA Grade 3 EP ISO Grade 100
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Syncon Mist Oil is a premium quality, synthetic, extreme-pressure (EP) gear lubricant developed for use in oil mist lubrication systems for enclosed industrial gear drives operating under extreme-temperature conditions. Syncon Mist Oil is formulated with synthetic polyalphaolefin (PAO) base oils, a misting agent and specially tailored additives that provide extreme-pressure properties plus rust and corrosion protection. It has outstanding oxidation resistance and thermal stability at high temperatures to minimize deposit formation, and has high load-carrying capacity for protection against scuffing and wear. The misting agent helps reduce fogging and stray mist.

Applications: Syncon Mist Oil is recommended for use in oil mist lubrication systems for:

  • Lightly to moderately loaded enclosed industrial gear drives with spur, helical, herringbone or bevel gears
  • Chain drives
  • Plain and rolling-element bearings in rolling, rod and wire mills
Syncon Mist Oil meets the requirements of the following industry specifications:
  • ANSI/AGMA Standard 9005-E02
  • U.S. Steel 224
Features/Benefits:
  • Outstanding oxidation resistance and thermal stability at high temperatures
  • Excellent low-temperature fluidity
  • High load-carrying capacity
  • Reduces stray mist
  • Low fogging tendency
  • Protects against scuffing and wear
  • Protects against rust and corrosion

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.862 g/cc
Density 7.18 lb/gal
Viscosity Measurement 141Index
Saybolt Viscosity at 100°F 477 SUS
Saybolt Viscosity at 210°F 72.2 SUS
Kinematic Viscosity at 40°C (104°F) 93 cSt
Kinematic Viscosity at 100°C (212°F) 13.2 cSt
Oxidative Stability 29.16 hourRPVOT; ASTM D2272
ASTM Color 0.50ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.22[mg KOH/g]; ASTM D974
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 250 kgASTM D2596
Four Ball Wear 0.330 mmScar Diameter; ASTM D4172
 
Thermal PropertiesOriginal ValueComments
Pour Point -36.0 °C
Flash Point 274 °CCOC
 
Descriptive Properties
Copper Corrosion1aASTM D130
Demulsibility10 minutes to passASTM D1401

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5235 / 198488

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.