MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Reynolds EpoxAmite® White; Hardener: 102 Medium Epoxy Laminating System is
Categories: Polymer; Thermoset; Epoxy

Material Notes: Product Overview: EpoxAmite™ White Epoxy Laminating System is an easy-to-use liquid epoxy system formulated for a wide variety of fabrication applications. EpoxAmite™ White Laminating System is low in viscosity, odorless and cures at room temperature. Cured epoxy displays exceptional physical and performance properties. It can be sanded, shaped, machined, drilled, tapped and painted. EpoxAmite™ White Laminating System can be used with reinforcements such as S-Glass, E-Glass, Kevlar and Carbon fibers for lay-up applications or composite parts. EpoxAmite™ White Resin can also be mixed with fillers such as fumed silica for gel coat applications. Urefil™ 3, Urefil™ 7 and other fillers can be added for fairing, filleting or bonding applications.

Applications:

  • Wet Lay-Up Lamination
  • General Bonding & Repair - Gel Coating
  • Barrier Coating
  • Thin-Section Casting
  • Water Proofing
  • Patching & Small Laminates
Advantages Include:
  • Easy-to-Use
  • Excellent Moisture Resistance - Low Viscosity
  • Non-blush Formula - Easy-to-Mix & Apply
  • Exceptional Physical & Performance Properties

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.23 g/cc1.23 g/ccASTM D-1475
Viscosity 2800 cP2800 cPMixed; ASTM D-2393
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585ASTM D-2240
Tensile Strength, Ultimate 38.6 MPa5600 psiafter 7 days at 73°F/23°C.; ASTM D-638
 212 MPa30700 psitesting conducted on a 6 ply/10 oz. laminate after 7 days at 73°F/23°C; ASTM D-638
Elongation at Break 1.2 %1.2 %ASTM D-638
Tensile Modulus 3.84 GPa557 ksiASTM D-638
Flexural Strength 57.6 MPa8350 psiafter 7 days at 73°F/23°C.; ASTM D-790
 218 MPa31600 psitesting conducted on a 6 ply/10 oz. laminate after 7 days at 73°F/23°C; ASTM D-790
Flexural Modulus 3.08 GPa446 ksiASTM D-790
Compressive Strength 82.46 MPa11960 psiASTM D-695
Compressive Modulus 0.0786 GPa11.4 ksiASTM D-695
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 56.0 °C133 °FHeat Deflection Temperature; ASTM D-648
 
Processing PropertiesMetricEnglishComments
Cure Time 120 min2.00 hourThin Film Working Time
 1200 - 1440 min20.0 - 24.0 hour
Pot Life 62.0 min62.0 minASTM D-2471
 
Descriptive Properties
ColorWhite
Mix Ratio100A:23Bby weight
Specific Volume22.5[in3/lb], ASTM D-792

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN191 / 296892

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.