MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Glyptal 1559 Alkyd Nitrocellulose Lacquer
Categories: Other Engineering Material; Ceramic/Metallic Coating

Material Notes: DESCRIPTION: GLYPTAL 1559 Gloss White Lacquer was designed or general purpose finishing of industrial products. This alkyd nitrocellulose lacquer has good color and gloss retention, good humidity resistance, and very good weather durability.

SUGGESTED USES: GLYPTAL 1559 is designed for use as a custom finish for industrial products. It is also suitable for finishing hospital and kitchen equipment as well as trucking equipment. Because of exterior durability, this paint is ideal for use on outdoor signs.

APPLICATION: GLYPTAL 1559 White Lacquer may be applied by spray or dip methods. When used to finish metal surfaces, it is preferable that a primer such as Glyptal 7920 be used first.

REDUCTION: For spray or dip application, thin 1559 Lacquer with approximately equal volume of G1514 Lacquer Thinner to 20-25 seconds using #2 Zahn Cup.

SURFACE PREPARATION: Surfaces to be painted should be dry and free from dirt, wax, grease, rust, and oil. Remove grease and oil by washing surface with mineral spirits. Allow surface to dry thoroughly. When painting over a glossy surface, reduce gloss by using fine sand paper or steel wool.

Information provided by Glyptal Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Flash Point <= 80.0 °F
 
Processing PropertiesOriginal ValueComments
Dry Time 0.500 hourAir Dry: Touch
 4.00 hourAir Dry: Hard
 
Descriptive Properties
ColorWhite
Coverage350 ft²/gal1 mil dried film
GlossHigh
RecoatOvernight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Unifrax Fiberfrax® Durablanket® 2600 Ceramic Fiber Insulator
Unifrax Fiberfrax® 970 Ceramic Fiber Paper
Glyptal 2600 Alkyd Nitrocellulose Lacquer
Glyptal 1276 Lacquer Cement
Chosun Refractories 1260PAPER Paper

PGLYPT909 / 209748

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.