MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Total PS CPDS 819 Flame Retardant Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Flame Retardant

Material Notes: POLYSTYRENE (PS) COMPOUND (CPDS) 819 is a high impact brominated flame retardant polystyrene. A combination of high flow and high heat stability gives excellent processability and reduced cycle times. PS CPDS 819 can be supplied in both natural and colored forms.

Main Characteristics:

  • Compliant with the European ECOLABEL (2009/300/EC),
  • DBDPE free,
  • Excellent UV stability,
  • High flow, high heat stability,
  • UL94 V0 @ 1.6 mm.

Applications: Covers for electrical equipment, TV covers, office automation.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity <= 1.13 g/cc<= 1.13 g/ccISO 1183
Water Absorption <= 0.10 %<= 0.10 %ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/in
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 200 °C
10 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133H
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 25.0 MPa3630 psiISO 527-2
Elongation at Break 40 %40 %ISO 527-2
Flexural Modulus 2.30 GPa334 ksiISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²180/1A
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 85.0 °C
@Load 5.10 kg
185 °F
@Load 11.2 lb
50°C per hour; ISO 306B50
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Black
 
Processing PropertiesMetricEnglishComments
Melt Temperature <= 260 °C<= 500 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Low Alloy Steel
Overview of materials for AISI 4000 Series Steel

PTOTAL896 / 130621

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.