MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Wefapress PETP Semi-crystalline thermoplastic polyethylene terephthalate
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: PETP is a semi-crystalline thermoplastic polyethylene terephthalate. This material features wear levels that are better than those of POM and also less moisture absorption than POM. PETP is especially suitable for complex precision parts. Properties: Withstands temperatures of >100°C for long periods of time, FDA-approved, Good sliding properties, High wear resistance, Conforms to EU 10/2011 (FSP variant), Excellent dimensional stability.

Applications: Components for the food industry, Components for pharmaceutical industry, Machine parts with a narrow tolerance range, Sliding profiles, slide bearings, slide rails. Industries: Conveyor systems and automation, Drinks and bottling industries, Mechanical and plant engineering, Food industry.

Information provided by Wefapress.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³DIN 53479
Moisture Absorption <= 0.200 %<= 0.200 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 85
@Time 15.0 sec
85
@Time 0.00417 hour
DIN 53505
Ball Indentation Hardness 140 MPa
@Time 30.0 sec
20300 psi
@Time 0.00833 hour
DIN ISO 2039 Teil 1
Tensile Strength 80.0 MPa11600 psiDIN 53455
Tensile Strength, Ultimate 80.0 MPa11600 psiDIN 53455
Elongation at Break 40 %40 %DIN ISO / R 527
Modulus of Elasticity 3.00 GPa435 ksiDIN 53457
1% Secant Modulus 1.00 MPa145 psiEU 1935/2004 - EU 10/2011 (FSP Quality)
Charpy Impact, Notched >= 0.400 J/cm²>= 1.90 ft-lb/in²DIN 53457
Coefficient of Friction 0.250.25
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C44.4 µin/in-°FDIN ISO 11359
Specific Heat Capacity 1.10 J/g-°C0.263 BTU/lb-°F
Thermal Conductivity 0.240 W/m-K1.67 BTU-in/hr-ft²-°F
Melting Point 255 °C491 °FDTA
Maximum Service Temperature, Air 75.0 °C167 °FDimensional Stability; DIN 53461
 100 °C212 °FContinuous Application Temp.
Minimum Service Temperature, Air -20.0 °C-4.00 °F
Flammability, UL94 HBHB
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWEFA937 / 243142

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.