MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ITW Permatex® Nickel Anti-Seize
Categories: Fluid; Lubricant

Material Notes: Products include thread lockers, sealants, gasket makers, cleaners and lubricants. Permatex® Nickel Anti-Seize Lubricant is a high temperature, high quality, heavy duty lubricant that resists galling and corrosion and reduces wear in heavy pressure applications. It contains tenacious metals, oils and graphite materials that cannot be burned away or removed by slow moving parts. This product withstands temperatures ranging from -65°F to 2400°F (-54°C to 1316°C). It is recommended for use where copper contamination must be avoided, under conditions of extreme pressure and temperature and with stainless steel, titanium and nickel alloys. OEM recommended.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
Viscosity 200000 cPbase
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 2400 °F
Minimum Service Temperature, Air -65.0 °F
Flammability Test 1.0NFPA 704
Flash Point 200 °F
 
Descriptive Properties
Chemical TypeMineral oil, nickel, graphite
ColorGrayPaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWP9163 / 239673

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.