MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos H00G-00 Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: A polypropylene homopolymer produced by Ineos utilizing catalyst technology. This material meets the Food and Drug Administration requirements of 21CFR 177.1520. Homopolymer H00G-00 meets certain automotive resin specifications.

Key Words: Homopolymer produced by unique catalyst technology
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.908 g/cc0.0328 lb/in³ASTM D792
Melt Flow 0.70 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.70 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9898ASTM D785
Hardness, Shore D 7474ASTM D2240
Tensile Strength at Break 22.1 MPa3210 psi2.0 in/min; ASTM D638
Tensile Strength, Yield 36.0 MPa5220 psi2.0 in/min; ASTM D638
Elongation at Break 120 %120 %2.0 in/min; ASTM D638
Elongation at Yield 12 %12 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 1500 MPa217000 psiASTM D790A
Izod Impact, Notched 0.518 J/cm0.970 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 5.10 kJ/m²2.43 ft-lb/in²Area; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 103 °C217 °FUnannealed; ASTM D648
Flammability, UL94 HBHB
 
Optical PropertiesMetricEnglishComments
Haze 69 %
@Thickness 1.27 mm
69 %
@Thickness 0.0500 in
ASTM D1003
Gloss 90 %90 %60°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
processBlow Molding
 Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem F006EC2 Homopolymer Polypropylene
Flint Hills P9G1Z-047 Polypropylene
Ineos H02C-00 Polypropylene Homopolymer
Braskem F008F Homopolymer Polypropylene
Ineos H11G-01 Polypropylene Homopolymer

PSOLL0 / 68246

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.