Sinkral® B9 ROMA is an extrusion grade ABS which exhibits excellent impact strength coupled with a high modulus. It also retains its excellent mechanical properties even after several re-extrusions and is therefore readily recycled. Applications: Extruded sheets requiring superior mechanical properties. Can also be added to recycled material to improve mechanical properties (post end user & extrusion scraps. Information provided by Versalis. |