MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Menzolit Menzolit® SMC 0421 Unsaturated Polyester UP
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: SMC 0421 is a low density premium Class-A SMC for on-line painted exterior body applications on cars. These compounds mould to light weight parts with excellent surface quality for on-line painted body panels at high paint bake temperatures (190- 200 °C). Moulded parts comply with all regulations of the automotive industry including low C-emissions. Surface defects like waviness, fibre patterns and orange peel are not existent with this product. To achieve the highest surface quality, we recommend that tool surfaces are mirror polished.

Information Provided by Menzolit

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.50 g/ccISO 1183
Water Absorption <= 0.50 %ISO 62
Linear Mold Shrinkage -0.000500 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 75.0 MPa
@Temperature 22.0 °C
25 mm flat samples, compression molded; ISO 527-4
Tensile Strength, Yield 75.0 MPa
@Temperature 22.0 °C
25 mm flat samples, compression molded; ISO 527-4
Elongation at Break 1.3 %ISO 527-4
Modulus of Elasticity 8.00 GPa25 mm flat samples, compression molded; ISO 527-4
Flexural Strength 150 MPa
@Temperature 22.0 °C
25 mm wide 100 mm long, flat samples; ISO 14125
Flexural Modulus 8.00 GPa
@Temperature 22.0 °C
25 mm wide 100 mm long, flat samples; ISO 14125
Compressive Yield Strength 80.0 MPaISO 14126
Poissons Ratio 0.30
Shear Modulus 3.10 GPain plane
Charpy Impact, Notched 7.00 J/cm²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohmIEC 60093
Dielectric Constant 4.0IEC 60250
Dielectric Strength 24.0 kV/mmIEC 60243-1
Dissipation Factor 0.010IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µm/m-°CISO 11359-2
Specific Heat Capacity 1.10 J/g-°C
Thermal Conductivity 0.700 W/m-K
Maximum Service Temperature, Air 165 °C
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °CISO 75-2
Minimum Service Temperature, Air -40.0 °C
Glass Transition Temp, Tg 200 °CISO 11357-2
Flammability, UL94 HB
@Thickness 3.00 mm
Oxygen Index 22 %ISO 4589-2
Glow Wire Flammability Index 750 °CIEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 145 - 155 °CCompression molding, matched metal die

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Menzolit Menzolit® SMC 0520 Unsaturated Polyester UP
Menzolit Menzolit® SMC 0500 Unsaturated Polyester UP
Menzolit Menzolit® SMC 0412 Unsaturated Polyester UP
Menzolit Menzolit® SMC 0390 Unsaturated Polyester UP
Menzolit Menzolit® SMC 0420 Unsaturated Polyester UP

PMENZ043 / 100777

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.