MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Wacker® Finish WT 1650 Silicone Fluid
Categories: Fluid; Polymer

Material Notes: Product description: WACKER® FINISH WT 1650 is a non reactive "functional silicone fluid".

Application: WACKER® FINISH WT 1650 is particularly suitable as active substance in softener formulations for the impregnation of fibers and textiles. WACKER® FINISH WT 1650 imparts a very soft, drapable, and elastic touch to woven and knitted fabrics. WACKER® FINISH WT 1650 is considered to be the best softening agent for PES-knit ware. WACKER® FINISH WT 1650 improves the wash-and wear properties and the crease recovery angle, sewability and tear strength and reduces abrasion loss. The effects are fast to washing and dry cleaning. WACKER® FINISH WT 1650 has only little effect on the degree of whiteness in a softener formulation. As a rule no adverse effect on the shade or color fastness properties of colored goods is observed.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 1000 cPdynamic
 
Descriptive Properties
Amine number0.6 ml 1 N HCl/g
Appearanceclear to slightly turbid fluid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9779 / 205308

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.