MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SunChemical Gwent C2100126D6 Carbon Graphite Ink
Categories: Fluid; Metal; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: This ink is designed for biosensor applications, it gives a good electrochemical response when tested with buffered Ferricyanide solutions. This product is based on a unique curing process that results in a low temperature formation of a thermosetting conductive coating that combines excellent chemical, solvent and abrasion resistance.
Screen Printing Equipment: semi-automatic, manual
Screen Types: stainless steel, polyester, mesh 156-230tpi
Substrate: polyester, PVC, polycarbonate or ceramic

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 42 - 45 %
@Temperature 150 °C
Viscosity 5160 - 9720 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
Haake VT 550 PK1.1°
Thickness 25.0 - 36.0 micronsCured, Printed through 230 stainless steel mesh with 13 micron emulsion
Storage Temperature 20.0 °Csealed container
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 31 - 95 ohm
@Thickness 0.0250 mm
Printed through 230 stainless steel mesh with 13 micron emulsion
 
Processing PropertiesOriginal ValueComments
Cure Time 60.0 min
@Temperature 150 °C
Shelf Life 6.00 Month
 
Descriptive Properties
Coverage cm2/g245.45Coverage through at 230ss screen, 13 micron emulsion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Potters Industries Conduct-O-Fil® SH230S33 Silver-Coated Hollow Glass Spheres
Parson Adhesives SONLOCK™ 3204 Pre-Applied Threadlocker Adhesives

WGELZ9007 / 139320

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.