MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.15 - 1.82 g/ccAverage value: 1.45 g/cc Grade Count:270
Filler Content 10.0 - 50.0 %Average value: 27.3 % Grade Count:37
Water Absorption 0.100 - 7.50 %Average value: 2.33 % Grade Count:102
Moisture Absorption at Equilibrium 0.170 - 6.00 %Average value: 1.57 % Grade Count:92
Water Absorption at Saturation 2.00 - 8.00 %Average value: 5.27 % Grade Count:47
Additive Loading 20.0 - 35.0 %Average value: 26.4 % Grade Count:9
Viscosity Test 150 cm³/gAverage value: 150 cm³/g Grade Count:3
Viscosity Number 140 cm³/gAverage value: 140 cm³/g Grade Count:4
Maximum Moisture Content 0.0500 - 0.200Average value: 0.100 Grade Count:3
Linear Mold Shrinkage 0.00100 - 0.0200 cm/cmAverage value: 0.00500 cm/cm Grade Count:208
 0.00300 - 0.00400 cm/cm
@Temperature 80.0 - 80.0 °C
Average value: 0.00333 cm/cm Grade Count:6
Linear Mold Shrinkage, Transverse 0.00200 - 0.0460 cm/cmAverage value: 0.00934 cm/cm Grade Count:93
 0.00600 - 0.0100 cm/cm
@Temperature 80.0 - 80.0 °C
Average value: 0.00867 cm/cm Grade Count:6
Melt Flow 1.00 - 53.6 g/10 minAverage value: 14.6 g/10 min Grade Count:29
Ash 20.0 - 30.0 %Average value: 25.7 % Grade Count:7
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 55.0 - 100Average value: 85.6 Grade Count:12
Hardness, Rockwell R 101 - 122Average value: 118 Grade Count:33
Hardness, Shore D 82.0 - 90.0Average value: 87.0 Grade Count:3
Ball Indentation Hardness 190 MPaAverage value: 190 MPa Grade Count:3
Tensile Strength, Ultimate 50.0 - 240 MPaAverage value: 129 MPa Grade Count:223
 30.0 - 145 MPa
@Temperature 60.0 - 150 °C
Average value: 78.6 MPa Grade Count:14
Tensile Strength, Yield 47.5 - 180 MPaAverage value: 120 MPa Grade Count:50
Elongation at Break 1.00 - 12.0 %Average value: 3.03 % Grade Count:240
 2.40 - 20.0 %
@Temperature 60.0 - 150 °C
Average value: 4.89 % Grade Count:14
Elongation at Yield 2.00 - 5.00 %Average value: 3.33 % Grade Count:10
 3.00 - 10.0 %
@Temperature 60.0 - 150 °C
Average value: 4.84 % Grade Count:6
Modulus of Elasticity 3.21 - 17.5 GPaAverage value: 8.86 GPa Grade Count:179
 0.220 - 11.5 GPa
@Temperature 60.0 - 150 °C
Average value: 5.24 GPa Grade Count:14
Flexural Yield Strength 68.0 - 380 MPaAverage value: 190 MPa Grade Count:193
Flexural Modulus 3.10 - 15.6 GPaAverage value: 7.83 GPa Grade Count:189
Compressive Yield Strength 26.9 - 148 MPaAverage value: 105 MPa Grade Count:4
Poissons Ratio 0.340 - 0.360Average value: 0.350 Grade Count:4
Izod Impact, Notched 0.270 - 1.50 J/cmAverage value: 0.787 J/cm Grade Count:107
 0.220 - 0.69407 J/cm
@Temperature -40.0 - -20.0 °C
Average value: 0.388 J/cm Grade Count:3
Izod Impact, Unnotched 0.374 - 8.54 J/cmAverage value: 6.52 J/cm Grade Count:27
Izod Impact, Notched (ISO) 3.00 - 20.0 kJ/m²Average value: 9.03 kJ/m² Grade Count:71
 6.00 - 11.0 kJ/m²
@Temperature -40.0 - -30.0 °C
Average value: 7.95 kJ/m² Grade Count:25
Izod Impact, Unnotched (ISO) 35.0 - 60.0 kJ/m²Average value: 44.9 kJ/m² Grade Count:9
 39.0 - 47.0 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 44.0 kJ/m² Grade Count:4
Charpy Impact Unnotched 2.00 J/cm² - NBAverage value: 5.95 J/cm² Grade Count:130
 2.00 - 9.50 J/cm²
@Temperature -40.0 - -20.0 °C
Average value: 5.52 J/cm² Grade Count:56
Charpy Impact, Notched 0.200 - 2.94 J/cm²Average value: 0.973 J/cm² Grade Count:153
 0.200 - 10.0 J/cm²
@Temperature -40.0 - -20.0 °C
Average value: 0.936 J/cm² Grade Count:47
Taber Abrasion, mg/1000 Cycles 24.0 - 29.0Average value: 25.7 Grade Count:3
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1000 - 1.00e+18 ohm-cmAverage value: 2.27e+16 ohm-cm Grade Count:121
Surface Resistance 2500 - 1.00e+16 ohmAverage value: 1.74e+14 ohm Grade Count:73
Dielectric Constant 3.00 - 5.50Average value: 3.91 Grade Count:56
Dielectric Strength 11.0 - 90.0 kV/mmAverage value: 40.2 kV/mm Grade Count:89
Dissipation Factor 0.00900 - 0.200Average value: 0.0449 Grade Count:38
Arc Resistance 130 secAverage value: 130 sec Grade Count:3
High Voltage Arc Resistance to Ignition (HVAR) 120 secAverage value: 120 sec Grade Count:3
Comparative Tracking Index 200 - 600 VAverage value: 498 V Grade Count:115
Hot Wire Ignition, HWI 30.0 - 120 secAverage value: 110 sec Grade Count:12
High Amp Arc Ignition, HAI 120 arcsAverage value: 120 arcs Grade Count:15
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.0 - 80.0 µm/m-°CAverage value: 33.0 µm/m-°C Grade Count:47
 19.0 - 30.0 µm/m-°C
@Temperature 35.0 - 55.0 °C
Average value: 23.8 µm/m-°C Grade Count:4
 19.0 - 30.0 µm/m-°C
@Thickness 2.00 - 2.00 mm
Average value: 23.8 µm/m-°C Grade Count:4
CTE, linear, Transverse to Flow 60.0 - 100 µm/m-°CAverage value: 76.3 µm/m-°C Grade Count:16
Specific Heat Capacity 1.40 - 1.50 J/g-°CAverage value: 1.45 J/g-°C Grade Count:4
Thermal Conductivity 0.317 - 0.340 W/m-KAverage value: 0.329 W/m-K Grade Count:7
Melting Point 253 - 305 °CAverage value: 260 °C Grade Count:112
Maximum Service Temperature, Air 90.0 - 260 °CAverage value: 155 °C Grade Count:58
Hot Ball Pressure Test 165 - 230 °CAverage value: 215 °C Grade Count:14
Deflection Temperature at 0.46 MPa (66 psi) 177 - 265 °CAverage value: 251 °C Grade Count:119
Deflection Temperature at 1.8 MPa (264 psi) 75.0 - 280 °CAverage value: 228 °C Grade Count:211
Vicat Softening Point 215 - 255 °CAverage value: 245 °C Grade Count:63
UL RTI, Electrical 65.0 - 150 °CAverage value: 118 °C Grade Count:18
UL RTI, Mechanical with Impact 65.0 - 140 °CAverage value: 104 °C Grade Count:18
UL RTI, Mechanical without Impact 65.0 - 150 °CAverage value: 117 °C Grade Count:18
Flammability, UL94 HB - 5VAGrade Count:243
Flame Spread 0.000 mm/minAverage value: 0.000 mm/min Grade Count:6
Oxygen Index 25.0 - 44.0 %Average value: 31.3 % Grade Count:43
Glow Wire Test 650 - 975 °CAverage value: 887 °C Grade Count:110
 
Processing PropertiesOriginal ValueComments
Processing Temperature 235 - 310 °CAverage value: 279 °C Grade Count:47
Nozzle Temperature 254 - 300 °CAverage value: 275 °C Grade Count:19
Melt Temperature 220 - 320 °CAverage value: 279 °C Grade Count:137
Mold Temperature 40.0 - 121 °CAverage value: 82.5 °C Grade Count:161
Drying Temperature 71.0 - 130 °CAverage value: 89.5 °C Grade Count:141
Moisture Content 0.0300 - 0.250 %Average value: 0.173 % Grade Count:74
Dew Point -40.0 - -17.8 °CAverage value: -19.6 °C Grade Count:12
Injection Pressure 3.50 - 138 MPaAverage value: 92.4 MPa Grade Count:59

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
Overview of materials for Nylon 66, Unreinforced
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
Overview of materials for Nylon 66, 10% Glass Fiber Filled
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced

O2520 / 78019

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.