MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chevron Phillips 7109T LLDPE Blown Film Resin, Hexene Copolymer  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: Resin Type: Hexene Copolymer

Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPE

Applications:Industrial Liners, Stretch Wrap, Garment Bags, Carrier Bags, Coextrusions

Processing Conditions: Extruder 6.35 cm. Screw L/D Ratio 24:1. Die Opening 0.1905 cm. Blow-Up Ratio 2:1.

Film properties below based on film thickness of 31.8 µm.

Data provided by Chevron Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccASTM D1505
Melt Flow 0.90 g/10 minCondition E; ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 560 %ASTM D882
Film Elongation at Break, TD 770 %ASTM D882
Secant Modulus, MD 0.250 GPaASTM D882
Secant Modulus, TD 0.310 GPaASTM D882
Coefficient of Friction 1.0ASTM D1894
Elmendorf Tear Strength, MD 420 g/milNotched; ASTM D1922
Elmendorf Tear Strength, TD 840 g/milASTM D1922
Dart Drop 4.70 g/micronF50; 1.5 in. dart/26 in. drop height; ASTM D 1709
Film Tensile Strength at Break, MD 53.0 MPaASTM D882
Film Tensile Strength at Break, TD 53.0 MPaASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 13 %ASTM D2457
Gloss 60 %at 45°. ASTM D 2457
 100 %at 60°. ASTM D 2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHEVV35 / 20431

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.