MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LyondellBasell Moplen RP410M HP Random Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Moplen RP410M HP is a controlled rheology medium modified polypropylene random copolymer. It does not contain slip and anti-blocking additives. It is produced with a non-phthalate based catalyst. Moplen RP410M HP is typically used for manufacturing cast films and BOPP films. Customers adopt this grade to manufacture the sealing layer of mono-material retortable films (low sealing temperature and good heat resistance), which can find their use in pouches for food applications. Moplen RP410M HP exhibits good processability and optical properties. This grade is supported for use in drinking water applications.

Availability: Africa-Middle East; Europe

Application: Bags & Pouches; Food Packaging Film; Lamination Film; Textile Packaging Film

Market: Flexible Packaging

Processing Method: BOPP; Cast Film

Attribute: Controlled Rheology; Good Heat Seal; Good Sealing Strength; High Clarity; Retortable

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183-1
Melt Flow 7.00 g/10 min
@Load 2.16 kg,
Temperature 230 °C
7.00 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 26.0 MPa3770 psiISO 527-1, -2
Tensile Strength, Yield 25.0 MPa3630 psiISO 527-1, -2
Elongation at Break >= 650 %>= 650 %ISO 527-1, -2
Elongation at Yield 14.0 %14.0 %ISO 527-1, -2
Flexural Modulus 0.850 GPa123 ksiISO 178
Charpy Impact, Notched  0.200 J/cm²
@Temperature 0.000 °C
0.952 ft-lb/in²
@Temperature 32.0 °F
ISO 179-1/1eA
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C158 °FUnannealed; ISO 75B-1, -2
Vicat Softening Point 137 °C279 °FA50; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9709 / 324644

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.