MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Permabond 792 Cyanoacrylate, Surface insensitive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: PERMABOND® 792 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers are also rapidly bonded. The fast cure minimizes the occurrence of frosting and fogging.

Cyanoacrylate adhesives are single component adhesives that polymerize rapidly when pressed into a thin film between parts. The moisture adsorbed on the surface initiates the curing of the adhesive. Strong bonds are developed extremely fast and on a great variety of materials. These properties make PERMABOND cyanoacrylates the ideal adhesives for high speed production lines.

Features & Benefits:

  • Extremely fast setting
  • Rapid development of high strength
  • Ease of use – no mixing or heat cure
  • Surface insensitive
  • 100% reactive, no solvents

Information provided by Permabond.

Key Words: A-46060C Type II, Class 2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccUncured
Viscosity 60 - 125 cP
@Temperature 25.0 °C
60 - 125 cP
@Temperature 77.0 °F
Uncured
Storage Temperature 2.00 - 7.00 °C35.6 - 44.6 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585ISO 868
Tensile Strength >= 20.0 MPa>= 2900 psiISO 6922
Adhesive Bond Strength 18.0 - 22.0 MPa2610 - 3190 psiISO 4587, Shear
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 25.0 kV/mm635 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°F
Thermal Conductivity 0.100 W/m-K0.694 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 82.2 °C180 °F
Minimum Service Temperature, Air -62.2 °C-80.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 0.0333 - 0.0500 min0.000556 - 0.000833 hourSteel, handling time
 0.0333 - 0.0500 min0.000556 - 0.000833 hourBuna N Rubber, handling time
 0.0333 - 0.0500 min0.000556 - 0.000833 hourPhenolic, handling time
 1440 min24.0 hourfull strength
 
Descriptive Properties
AppearanceColorlessUncured
Maximum Gap Fill (mm)0.15
Strength Retention10% at 150°CRelative to 0°C
 100% at 0°CRelative to 0°C
 50% at 100°CRelative to 0°C
 75% at -50°CRelative to 0°C
 90% at 50°CRelative to 0°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Ethyl Cellulose, Molded
Rotuba 860H Ethyl Cellulose
Rotuba 860H2 Ethyl Cellulose
Rotuba 860S Ethyl Cellulose
Overview of materials for Acrylic, General Purpose, Molded

PPERMA38 / 56146

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.