MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Return Polymers RP1110 100% reycle PVC
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Vinyl (PVC); PVC, Molded

Material Notes: 100% recycled WHITE PVC pulverized into a 20 mesh powder and blended in large quantities to ensure consistency. Primarily used in fence, window, and siding applications with or without a capstock layer and processed by single and or twin screw extrusion.

Information provided by Return Polymers Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.42 g/ccASTM D-792
Bulk Density 31.0 lb/ft³ASTM D1895
Particle Mesh Size 20 Mesh3% retention
 120 Mesh97% retention
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 7172 psi
@Thickness 3.00 mm
Type I, 2 in/min; ASTM D 1990
Tensile Impact Strength 80.0 ft-lb/in²
@Thickness 3.00 mm
Type S; ASTM D1822
Dart Drop Total Energy 4.00 ft-lb/mil70 F, 8# wt, ½” conical tup. Maximum value on a 2" strip recorded; ASTM D4226
 
Electrical PropertiesOriginal ValueComments
Hot Wire Ignition, HWI 60 - 119 secASTM D3874
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 160 °FASTM D 648-85
Flammability, UL94 V-0
@Thickness 3.00 mm
 
Descriptive Properties
ColorWhite (L > 90)CIELab, D65, 10 degree observer or visual
FormPulverized Powder / Pellet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRETURN001 / 238935

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.