MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M 9475LEB High Strength Double Coated Tape with Adhesive 300LSE
Categories: Polymer; Adhesive

Material Notes: 3M™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acrylic adhesive also provides excellent adhesion to surfaces contaminated lightly with oil typically used with machine parts.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 12.7 microns0.500 milCarrier
 50.8 microns2.00 milFaceside Adhesive
 50.8 microns2.00 milBackside Adhesive
 88.9 microns3.50 milCaliper
 114 microns4.50 milTotal Thickness
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.49303 kN/m2.8125 pliStainless Steel, 180° peel, 2 mil Al foil backing, 15 min RT, Faceside; ASTM D3330
 0.657 kN/m3.75 pliGlass, 90° peel, 2 mil Al foil backing, 72 hr RT, Faceside; ASTM D3330
 0.657 kN/m3.75 pliPolypropylene, 90° peel, 2 mil Al foil backing, 72 hr RT, Faceside; ASTM D3330
 0.7669 kN/m4.375 pliStainless Steel, 180° peel, 2 mil Al foil backing, 72 hr RT, Faceside; ASTM D3330
 0.7669 kN/m4.375 pliPolypropylene, 90° peel, 2 mil Al foil backing, 72 hr RT, Backside; ASTM D3330
 0.7669 kN/m4.375 pliStainless Steel, 180°, 2 mil polyester as backing, 72 hr RT, Faceside; ASTM D3330
 0.7669 kN/m4.375 pliStainless Steel, 180° peel, 2 mil Al foil backing, 15 min RT, Backside; ASTM D3330
 0.82172 kN/m4.6875 pliGlass, 90° peel, 2 mil Al foil backing, 72 hr RT, Backside; ASTM D3330
 0.877 kN/m5.00 pliStainless Steel, 180°, 2 mil polyester as backing, 72 hr RT, Backside; ASTM D3330
 0.93128 kN/m5.3125 pliABS, 90° peel, 2 mil Al foil backing, 72 hr RT, Faceside; ASTM D3330
 0.9861 kN/m5.625 pliStainless Steel, 180° peel, 2 mil Al foil backing, 72 hr RT, Backside; ASTM D3330
 0.9861 kN/m5.625 pliStainless Steel, 180° peel, 2 mil Al foil backing, 72 hr 70°C, Faceside; ASTM D3330
 0.9861 kN/m5.625 pliABS, 90° peel, 2 mil Al foil backing, 72 hr RT, Backside; ASTM D3330
 1.1504 kN/m6.5625 pliStainless Steel, 180° peel, 2 mil Al foil backing, 72 hr 70°C, Backside; ASTM D3330
 1.31 kN/m7.50 pliPolycarbonate, 90° peel, 2 mil Al foil backing, 72 hr RT, Faceside; ASTM D3330
 1.31 kN/m7.50 pliPolycarbonate, 90° peel, 2 mil Al foil backing, 72 hr RT, Backside; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.0 °C199 °FLong term
 149 °C300 °FShort term
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Liner#83 Polycoated Kraft

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM33276 / 168023

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.