MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
MRC Polymers NAXALOY 770 Polycarbonate/ABS blend
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: NAXALOY 770 is a high impact Polycarbonate/ABS blend. This material is available in black, natural, and custom colors. It is typically used for automotive interior/exterior covered & painted applications.

Information provided by MCR Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/ccISO 1183
Melt Flow 21 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 51.0 MPaISO 527
Elongation at Yield 4.5 %ISO 527
Flexural Strength 70.0 MPaISO 178
Flexural Modulus 2300 MPaISO 178
Izod Impact, Notched (ISO) 23.0 kJ/m²
@Temperature -31.0 - -27.0 °C
ISO 180
 48.0 kJ/m²
@Temperature 21.0 - 25.0 °C
ISO 180
Charpy Impact, Notched 23.0 kJ/m²
@Temperature -32.0 - -28.0 °C
ISO 179
 53.0 kJ/m²
@Temperature 21.0 - 25.0 °C
ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 103 °Cunannealed; ISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MRC Polymers NAXALOY™ 770 ABS + PC Alloy
MRC Polymers NAXALOY 770GF10 Polycarbonate/ABS blend

PMRC5005 / 217591

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.